Thursday, May 29, 2014

[MW:20931] Re: Qualify Non Nace Material To Nace

If the steel is for new construction and you have material available then run the standard SSC and HIC testing for full qualification and ensure that the welding procedure is qualified to meet NACE MR 0175 / ISO 15156.  If it is already in service then review the weld procedure to confirm that it was done per NACE MR 0175 / ISO 15156 and/or measure the hardness of the weld and HAZ to ensure that is below the maximum hardness allowed per the NACE MR 0175 / ISO 15156 requirements of Table A.1 of NACE MR 0175 / ISO 15156-2

On Friday, May 23, 2014 2:00:20 AM UTC-5, Ri@z wrote:
Dear All,

I hav SA 516 gr 60 , Non nace material. Now my question is " What Is the Procedure or test requirement to make it NACE "



Riaz


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...