RE: [MW:20924] Use of ER 320 LR instead of ERNiCrMo-18 for Alloy 20 (UNS 08020)

Hello Jignesh,
 
This is the correct table follow (Ref RP-582-2009).ER 320LR is the default welding consumable for welding alloy-20.
 
Alloy-20 is no different than any other Higher grade or super austenitic stainless steels, hence weldability issues could be similar.
 
Thanks.
 
Pradip Goswami, P.Eng,IWE
Welding & Metallurgical Specialist
Ontario, Canada
pradip_goswami@yahoo.ca
 



El Miércoles, 28 de mayo, 2014 7:27 A.M., Jignesh Desai <jignesh.desai.met@gmail.com> escribió:


Can some one share his/her experience for the welding of SB463 UNS 08020? i.e. for welding of butt welds what shall be consumables?
As per API 582 Table B2- ER 320LR for overlay on CS/LAS & as per ASME Sec IIC, SFA 5.11/5.14 ERNi Cr Mo-18.

Regds/Jignesh
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.




--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...