I was told there is equipment which can be used for stress relief, particularly helpful when coming to SS welding when PWHT is not a good option. This must be done during the welding process, not post welding like PWHT.

 

For welding being carried out with CS & LA materials, it can achieve approx. 90% of what a PWHT can do if it be being used correctly. For welding being carried out with SS materials, it should able to achieve the same level of stress relief like CS/LA materials.

 

Let me know if anyone have any interest as demonstration can be arranged.

 

 

Thanks,

KL Chung

KTM Taiwan.

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Arunachalam A
Sent: Wednesday, 28 May, 2014 11:22 PM
To: materials-welding@googlegroups.com
Subject: Re: [MW:20924] PWHT for stainless steel weld joint

 

If you carry out the PWHT, then MDMT for the vessel is reduced to Minus 29 Deg C.

 

Regards,

 

 

On 27 May 2014 06:45, Ghafor Mohamad <ghaformohamad@gmail.com> wrote:

Control the interpass and heat input

Thanks
Ghafor Mohamad
SQE Alstom

On May 27, 2014 10:42 AM, "Raneesh.PK" <pkraneesh@gmail.com> wrote:

Dear all

 

As we know very well pwht is restricted for stainless steel   weld joint due to formation of chromium carbide(Senzitaion)

 

My question is how to reduce the weld stress of  stainless steel weld joint.

 

 Regards,

 

RANEESH.PK               

 

--
To post to this group, send email to
materials-welding@googlegroups.com
To unsubscribe from this group, send email to
materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at
http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to
materials-welding+unsubscribe@googlegroups.com.
For more options, visit
https://groups.google.com/d/optout.

--
To post to this group, send email to
materials-welding@googlegroups.com
To unsubscribe from this group, send email to
materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at
http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to
materials-welding+unsubscribe@googlegroups.com.
For more options, visit
https://groups.google.com/d/optout.




--

Arunachalam.A,

Abu Dhabi

00-971-50-5257122

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...