[MW:20917] Re: Welding of SS 304H to P-91

Dear Sir
As per literature cited by me especially Nickel Development Institute, I fully agree that Er NiCr3 is the best filler wire, however as per EIL Specification we are using ER309 as filler and E309-15/16 as electrode, with Preheating of 205 deg C and PWHT (732-760 deg C). what are the probable problems that can be associated with selecting this filler, as it is a well know fact that DMW for P-91 are one of the probable causes of failure. Kindly guide me with respective to literatures available
regards
Arunabh 
Engineers India Limited

On Tuesday, May 27, 2014 4:42:10 PM UTC+5:30, ARUNABH BERA wrote:
Dear All

Kindly clarify the doubts:
Sir in Ethylene Cracker Furnace at one of the Petrochemical Plant, we have a hook-up between P-91 and SS304H. Here we are using ER309 as the filler.
Is it acceptable, if not what can be the probable problems associated with the filler selection and what are the solutions 

Regards
Arunabh
Engineers India Limited

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...