RE: [MW:20871] Thickness of Blind Flange for Hydrotest

Hello,

 

You can search for more details in ASME B16.48

 

The dimensions for blinds (thickness, inside/outside diameter, etc) are in function of #ANSI, NPS and face type of your flange

 

In section 6 of ASME B16.48, specifies that blind material shall be accordance of ASME B16.5, which means that you must consider flange material too.

 

Regards

 

Miroslav Tadic
Ingeniero  de Integridad
CEE
Producción - Mantenimiento
YPFB Chaco S.A.

De: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] En nombre de Raja M
Enviado el: viernes, 23 de mayo de 2014 15:13
Para: materials-welding@googlegroups.com
CC: muthukumar_bemech@yahoo.com
Asunto: [MW:20868] Thickness of Blind Flange for Hydrotest

 

Dear Experts,

 

Please Explain me in detail about How to Calculate Thickness of Blind Flange for Hydrotest.

 

Note : I already read it in ASME B31.3 section 304.5.2, but still not clear.

 

Regards,

Raja.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.


______________________________________________________________________

La información contenida en este mensaje es privada y confidencial. Si usted no es el destinatario del mismo, queda notificado por este medio que está prohibido revelar, copiar o distribuir esta información. Si ha recibido este mensaje por error, por favor notifique al remitente en forma inmediata y proceda a borrarlo de su sistema. Muchas gracias.

The information contained in this message is private and confidential, intended only for the use of the individual or entity to whom it is addressed. If you are not the intended recipient, you are hereby notified that any disclosure, copying, or distribution is strictly prohibited. If you have received this message in error, please notify us immediately by responding to this email and then delete it from your system. Thank you.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...