Dear Sirs
As per the EIL Spec requirement, we are using ER-309 as filler and capping with E309-15/16. Preheating requirement only on P-91 Side: 205 deg C and PWHT 732 to 760 deg C. As per varios literature cited by me, especially literatures by Nickel Development Institute, i fully agree that ER-Ni Cr 3 is the best option. My question is that can using ER309 as a filler can lead to complications and failures. because DMW between P-91 are most prone to failures and i request experts to kindly throw light on this issue

On Tuesday, May 27, 2014 4:42:10 PM UTC+5:30, ARUNABH BERA wrote:
Dear All

Kindly clarify the doubts:
Sir in Ethylene Cracker Furnace at one of the Petrochemical Plant, we have a hook-up between P-91 and SS304H. Here we are using ER309 as the filler.
Is it acceptable, if not what can be the probable problems associated with the filler selection and what are the solutions 

Regards
Arunabh
Engineers India Limited

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...