Wednesday, May 21, 2014

RE: [MW:20858] GRE pipe

My opinion refer to manufacture recommendations


Sent from Samsung Mobile



-------- Original message --------
From: "R.N" <maestro.rn@gmail.com>
Date: 21/05/2014 12:24 AM (GMT+08:00)
To: materials-welding@googlegroups.com
Subject: [MW:20857] GRE pipe


Dear All, please share your opinions

GRE pipes damaged at few location after hydrotest. Damaged location repaired. Contractor proposal is carry out test with operating pressure.
Question:
1. Is normal to test with operating pressure? Damaged GRE pipes in particular
2. Is it advisable to use such kind of fixed GRE pipe on site even after testing?

Regards

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...