Re: [MW:20875] WPQ for SS to Inconel Welding

Yes I have old PQR for the same. Problem is crater crack only in the root joint and not in any subsequent pass.

On May 24, 2014 1:13 PM, "srinivasu" <srinivasu.mech@gmail.com> wrote:

I understood that you're qualifying a welder for F No.5 & F No.43

Your approach is good, but do you have any qualified procedure for your the below combinations
1) P No.8 to P No.8 with F No.5 electrode?
2) P No.8 to P No.8 with F No.43 electrode?
Because for welder qualification WPS is required as per ASME sec. IX

On Apr 23, 2014 6:47 PM, "Hrushikesh Sangamnerkar" <hrushi612@gmail.com> wrote:

Dear all,

Plate thickness 14 mm
Plate material SA 240 TYPE 304L
Joint Single V groove joint
Can I qualify welder for SS and inconel ( for F-No) in the same joint?
Weld deposited thickness 7mm (for SS ) and 7mm (for inconel).
I have heard that SS cannot be welded on Inconel but vice versa is  possible i.e. Inconel on SS.
If yes how? And if answer is No then how?
Is there any metallurgical change involved in this?

Kindly help.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...