Friday, May 30, 2014

RE: [MW:20935] Pressure Equipment Directive(PED) - Impact Testing

You should refer to the PED Guidelines (make a Google search on that), which is a 255 page document from the EU Commission.

It does not state directly the 27J, but 27J is a common used criteria in European materials (EN materials). Also your WPS’s should be qualified to show compliance with that requirement, but that will come automatically because your WPS’s will need to address that they comply with PED 97/23/EC.

There are no impact test requirements on austenitic stainless steel – se guidelines.

 

You will find in the guidelines, that you need to have “Particular Material Assessments” (PMAs) made for non-European Materials, these should be verified by your selected Notified Body for the CE-marking.

 

For information: It is rather limited what your Notified Body may guide; their role is not to guide but to verify (and basically they cannot verify that they guided correctly themselves).

 

 

Yours sincerely

Kristian Lund Jepsen

 

M. Sc. Mech. Eng.

Senior Chief Consultant

Piping & Mechanical

 

D +45 - 51617324

M +45 - 23402936

________________________________________

 

Ramboll

Willemoesgade 2

DK-6700 Esbjerg

Denmark

 

DK reg.no. 35128417    

 

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Bhave, Suyog
Sent: 29. maj 2014 11:27
To: materials-welding@googlegroups.com
Subject: RE: [MW:20930] Pressure Equipment Directive(PED) - Impact Testing

 

Thank you for the reply.

If anyone have more information regarding where exactly the impact testing values are specified in PED and are these differ as per material.

I know the directive PED 97/23/EC, however the requirements are very general.

 

Is there any BV member of our group can guide me in detail. Thanks.

 

Best Regards,

Suyog Bhave

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of veera raghava kommisetti
Sent: Wednesday, May 28, 2014 17:28
To: materials-welding@googlegroups.com
Subject: Re: [MW:20911] Pressure Equipment Directive(PED) - Impact Testing

 

PED allows use of ASME code for design and construction and as such rules of ASME applies for Impact.

You can get additional requirements for compliance to PED in EC directive. Notified bodies will guide you in this respect.

 

On Wed, May 28, 2014 at 10:33 AM, Bhave, Suyog <Suyog.Bhave@petrofac.com> wrote:

Dear All,

 

I am currently working on project located at UK which requires compliance to PED (Pressure Equipment Directive) norms.

Can anybody have reference where I could find the details of PED related to PIPING engineering.

 

Also, is there any impact testing criteria specified in PED which is different than American codes.

 

Thanks in advance for your help.

 

Best Regards,

Suyog Bhave

This message, including any attachments, may contain confidential and privileged information for the sole use of the intended recipient(s). Review, use, distribution or disclosure by others is strictly prohibited. If you are not the intended recipient, or authorised to receive information on behalf of the recipient, please contact the sender by reply email, and delete all copies of this message. While we have taken reasonable precautions to ensure that this message and any attachments are free from viruses, we cannot guarantee that they are virus free and accept no liability for any damage caused by this message or any attachments. Messages sent or received through our networks may be monitored to ensure compliance with the law, regulation and/or our policies.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

This message, including any attachments, may contain confidential and privileged information for the sole use of the intended recipient(s). Review, use, distribution or disclosure by others is strictly prohibited. If you are not the intended recipient, or authorised to receive information on behalf of the recipient, please contact the sender by reply email, and delete all copies of this message. While we have taken reasonable precautions to ensure that this message and any attachments are free from viruses, we cannot guarantee that they are virus free and accept no liability for any damage caused by this message or any attachments. Messages sent or received through our networks may be monitored to ensure compliance with the law, regulation and/or our policies.

--
To post to this group, send email to
materials-welding@googlegroups.com
To unsubscribe from this group, send email to
materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at
http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...