Re: [MW:16651] ASTM A514 TYPE T-1

Dear All

Now it is clear for ASTM 514 T-A we can use 11018-M or 12018-M 

But for Pushes we will use ALLOY 4140 can you tell me the specification of this alloy and what is the electrode to weld the plates ASTM 514 T-1 with this alloy 4140 

Regards,
Hani Alfe


From: c sridhar <sridhar305@yahoo.com>
To: "materials-welding@googlegroups.com" <materials-welding@googlegroups.com>
Sent: Wednesday, January 30, 2013 9:24 PM
Subject: Re: [MW:16640] ASTM A514 TYPE T-1

 

Mr. HA,

ASTM A 514  is a high-strength quenched and tempered plate for structural and pressure vessel applications.
It is also known asT-1 steel.  Consumables to weld it process wise are:

 
SMAW
A5.5/A5.5M-2005
E11018M or E12018M
GMAW
A5.28/A5.28M-2005
Solid electrodes ER 110S-1 and  ER120S
FCAW
A5.29/A5.29M-2005
E11XT1-K3C and -K3M
E11XT5-K3C and -K3M
 
 
Sridhar.
---------------------------------------------------------------------------------------------------------------------------------------------------------------------------------

From: hany alfy <hanyon_alfy@yahoo.com>
To: "materials-welding@googlegroups.com" <materials-welding@googlegroups.com>
Sent: Wednesday, 30 January 2013 1:06 PM
Subject: [MW:16635] ASTM A514 TYPE T-1



Dear All

We need to fabricate one mechanical Grab plates are grade ASTM A514 TYPE T-1
Which electrode we can use for welding

Regards,
H.A
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 


No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...