Wednesday, January 30, 2013

Re: [MW:16642] Current/Voltage Requirement for wire 1.6mm for GTAW welding.


You have not provided complete details like :
Base material, Type of joint, thickness, etc..
 
However for 1.6mm TIG filler wire you can use:
@ 80-140 A,
10-20V
For CS: 250 degrees C interpass temp and for SS :175 degrees C max.
 
Regards
 
Prem Nautiyal
9769316004
 

--- On Wed, 1/30/13, Anant Pandit <anant0106@gmail.com> wrote:

From: Anant Pandit <anant0106@gmail.com>
Subject: [MW:16625] Current/Voltage Requirement for wire 1.6mm for GTAW welding.
To: materials-welding@googlegroups.com
Date: Wednesday, January 30, 2013, 11:55 AM

Dear Experts,

i want information regarding GTAW welding. I am going to use 1.6mm filler wire, can anybody tell what temp/current/voltage to be maintain..

its urgent... please give your valluable reply...

Regards,

ANANT D PANDIT
For SAFESS QUALITY MGMT PVT. LTD.
PUNE.
MOBILE NO.-: +919604348931
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...