Wednesday, January 23, 2013

[MW:16574] ASTM A516 Gr.70 normalizing

 

Dear All

 

I need to know how can understand that ASTM A516 Gr.70 is normalized or not?

 

Somebody told me:

 “according to clause 5.3 of ASTM A516 standard (attached), when we apply charpy impact test on a material and it pass the impact test successfully, we can say the material is surly normalized but if the material can’t pass the impact test, we shall apply metallographic test to understanding if the material is normalized.

 

And somebody said me:

“we have just 1 way to know that is the material normalized or not. And its metallographic test.”

 

M. Farhang

 

 

 

 

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...