[MW:16609] Stress relieving & Oxidation on titanium PQR

Dear Experts,

I have Qualified PQR with below deatils

Material: Titanium
Process: GTAW
Heat treatment done twice one is for stress relieving (600deg.C, 1hr soaking, furnace cooling) & other is for Oxidation( 750deg.C, 3hrs soaking, furnace cooling) on same PQR test cupon as per ASME sec.IX

Now my question is, can i write two WPS with separate HT's by having back up of above PQR

as one is with stress relieving & other is with Oxidation.

Request to send me the reply at the earliest with some back up like referance documents if any


Regards
Prasu

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...