Dear sir,

 

You are going to weld on CS or SS, Generally interpass temp is approx 190 c but again based on group of material.

Regarding about welding parameters you can refer an welding supplier cartoon & documents  for setting electrical parameter ,generally vary in root pass ,hot pass & Capping. Also based on the travel speed.

 

Heat input = v*I/ travel speed.

 

Regards

 

Dinesh

Pune @ desk of dubai

 

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Anant Pandit
Sent: Wednesday, January 30, 2013 10:26 AM
To: materials-welding@googlegroups.com
Subject: [MW:16625] Current/Voltage Requirement for wire 1.6mm for GTAW welding.

 

Dear Experts,

 

i want information regarding GTAW welding. I am going to use 1.6mm filler wire, can anybody tell what temp/current/voltage to be maintain..

 

its urgent... please give your valluable reply...

 

Regards,

 

ANANT D PANDIT

For SAFESS QUALITY MGMT PVT. LTD.

PUNE.

MOBILE NO.-: +919604348931

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...