Re: [MW:16617] Titanium to SS Welding


Titanium is not weldable to any Fe based materials.

It is only weldable to Hafnium, zirconium & Tantalum.

Regards,

Zakir Ali.


From: Craig Wesson <gr8fulone@gmail.com>
Sent: Fri, 25 Jan 2013 15:08:53
To: materials-welding@googlegroups.com
Subject: Re: [MW:16595] Titanium to SS Welding
cannot be done to my knowledge

Craig Franklin Wesson, Jr.
4805 Auburn Drive North    M A P
Mobile, AL 36618
cell  336-567-8774
View my LinkedIn profile
gr8fulone@gmail.com

   Please consider the environment before printing this email.
<><><><><><><><><><><><><><><><><><><><><><><><><><><><><><><><><><><><><><><><><><>
This message is confidential, intended only for the named recipient(s), and may contain information that is privileged or exempt from disclosure under applicable law.  If you are not the intended recipient(s), you are notified that the dissemination, distribution or copying of this message or any attached files is strictly prohibited. If you receive this message in error, or are not the named recipient(s), please notify the sender at the e-mail address above and discard this e-mail with any attached files immediately.

At the time of transmission, this email and any attachments are believed to be free of any virus or other defect, which might affect any computer system.  It is the responsibility of the recipient to check that it is virus-free at the time of receipt.  The sender accepts no responsibility or liability for any loss, injury, damage, cost, or expense arising in any way from receipt or use thereof by the recipient.

Thank you.

<><><><><><><><><><><><><><><><><><><><><><><><><><><><><><><><><><><><><><><><><><>


On Thu, Jan 24, 2013 at 6:10 AM, Noushad cp <ncp.clt@gmail.com> wrote:
Dear all

Please guide me,Which filler wire is use for SS to Titanium weld using
GTAW Process.


Noushad

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm

The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 


Catch India as it happens with the Rediff News App. To download it for FREE, click here

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...