Re: [MW:16571] P11 alloy steel Grade Material - PWHT scope

PWHT after welding is advisable for better properties.


From: Zakaria ghrab <zakaria.ghrab@gmail.com>
To: materials-welding@googlegroups.com
Sent: Wednesday, January 16, 2013 1:22 PM
Subject: [MW:16522] P11 alloy steel Grade Material - PWHT scope


Dear experts,

  I have one doubt.

We have P11 alloy grade material pipe, size 8" SCH 80,  thickness = 12.7 mm. So according ASME construction code PWHT is not mandatory.

For the same piping, we had one non conformance (pipe damage before installation). To release and close, client request to confirm thickness and dimensional check. We get for thickness measurement around 15 mm for all pipie lenght.

So, now client request to perform PWHT for welding joints related.

ISO Dwg mention 8" SCH 80.

How we can release ?


Regards.
--
زكرياء غراب
GHRAB Zakaria
+212606588856
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 


No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...