Re: [MW:16592] Titanium to SS Welding

There is no compatable consumables to weld Titanium to SS or any other discimilar metal by GTAW or SMaw
Regards
 
Hegde P.B.
----- Original Message -----
From: Noushad cp <ncp.clt@gmail.com>
To: materials-welding <materials-welding@googlegroups.com>
Cc:
Sent: Thursday, 24 January 2013 5:40 PM
Subject: [MW:16587] Titanium to SS Welding

Dear all

Please guide me,Which filler wire is use for SS to Titanium weld using
GTAW Process.


Noushad

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm

The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.


No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...