Controlling factor for PWHT temp  is CS and not SS  and we have heat treat as per ASME code UCS 56 or any applicable code
 
Regards
 
Hegde Prakash
----- Original Message -----
From: sevak hiren <hirensevak80@gmail.com>
To: "materials-welding@googlegroups.com" <materials-welding@googlegroups.com>
Cc:
Sent: Thursday, 24 January 2013 12:04 PM
Subject: [MW:16587] PWHT Temperature for welding CS To SS

Dear Experts,

Kindly suggest what should be the PWHT Temperature after welding of
following dissimilar materials.

SA 516 Gr.70 To SA 240 Gr.304

Regards

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm

The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.


No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...