Dear Farhang,

Based on my experience in laboratory, in some cases metallographic microstructures could not show the material whether normalized or not because this type of heat treatment will not affect microstructure as much as other heat treatments e.g. annealing. However in some cases we could see normalized microstructure clearly. The big problem is we have no judgment base for differing between normalized or non-normalized microstructures for different kind of materials.

I think because of that, standards based their qualifications on impact test (we have keep in mind that normalizing will improve toughness properties, I mean the subject is toughness not the normalizing by itself). So if you test a material and qualify for impact, you can assume it as normalized material or a material treated at least equal to normalizing.

 

Regards


On Wed, Jan 23, 2013 at 6:17 AM, M2M <hyperm2m@gmail.com> wrote:

 

Dear All

 

I need to know how can understand that ASTM A516 Gr.70 is normalized or not?

 

Somebody told me:

 "according to clause 5.3 of ASTM A516 standard (attached), when we apply charpy impact test on a material and it pass the impact test successfully, we can say the material is surly normalized but if the material can't pass the impact test, we shall apply metallographic test to understanding if the material is normalized.

 

And somebody said me:

"we have just 1 way to know that is the material normalized or not. And its metallographic test."

 

M. Farhang

 

 

 

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 



--
M. Shokri Arfaei
International Welding Engineer (IWE)
ASNT NDT Level III
ISA - STRI - Metallurgy Lab. Manager
Tel: +98-21-66282127
Fax: +98-21-66282779
 
Please don't print this e-mail unless you really need to. BeGreen!

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...