Saturday, June 30, 2012

Re: [MW:14725] carburization of furnace tubes

Consult an Eddy current Testing guy, may be it will help.

--- On Sat, 30/6/12, ags 36681 <ags1280@gmail.com> wrote:

From: ags 36681 <ags1280@gmail.com>
Subject: [MW:14724] carburization of furnace tubes
To: "materials-welding" <materials-welding@googlegroups.com>
Date: Saturday, 30 June, 2012, 6:54 PM

Dear friends,

we recently changed the ethane furnace tubes after service in 4 years,
now we are planning to segregate the healthy tubes & return  bends
from used/removed lot to re-use in future if needed. Material of the
tube/bend is 25Cr/35Ni/Nb+Micro.

We can check visually for cracks, thinning, bowing etc. UT is not
feasible, because there is some sort of rough coating over it.

How about the field metallography for carburization?

thanks a lot to all dear friends.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...