Skip to main content

Re: [MW:14714] Preheating Requirements For HOT TAPPING OF LPG PIPE LINES

To prevent HAZ hardness increase & HAZ crack
Regards,
Kavin Murugam
0126159644
 

From: Mohamed Elsayed ( BTG) <MElsayed@ccc.ae>
To: materials-welding@googlegroups.com
Sent: Tuesday, June 26, 2012 7:41 PM
Subject: [MW:14693] Preheating Requirements For HOT TAPPING OF LPG PIPE LINES

 
Dear Friends,
 
Could you please tell me , in Preheating process for Hot tap as per Shell DEP 30.10.60.30-Gen. (WELDING ON PRESSURISED PIPES (AMENDMENTS/SUPPLEMENTS TO ANSI/API RP 1107)) December 1998, Clause 4.8 (b) and (c) PREHEATING AND INTERPASS TEMPERATURE)
why we are increasing the temp. to 250 °C , then decreasing to 150 °C  before starting the welding and why the time taken for 250°C to cool to 150 °C shall be recorded
 
4.8 PREHEATING AND INTERPASS TEMPERATURE
(b) Longitudinal groove welds:
 
Prior to the commencement of welding, both seams shall be heated simultaneously to 250 °C over a minimum band width of twice the thickness of the fitting either side of the weld preparation. After welding has commenced, the preheat maintenance temperature shall be 150 °C.
 
(c) Circumferential fillet welds
With the fitting in position on the live pipeline, a minimum length of 300 mm of the weld zone shall be preheated to 250 °C. The temperature of the run pipe within this zone shall be monitored and the time taken for the zone to cool to 150 °C shall be recorded. This recorded time shall define the time limits between the cessation and the re-commencement of preheat during welding for the deposition of the first two layers of the weld metal including the buttering runs on the run pipe. Thereafter, the temperature shall be monitored so that welding does not occur when the weld zone is at a temperature of less than 150 °C.
 
 
Best Regards,
Mohamed El-Sayed
 
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.


Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...

The Schaeffler and Delong diagrams for predicting ferrite levels in austenitic stainless steel welds

Introduction Ferrite is important in avoiding hot cracking in during cooling from welding of austenitic stainless steels. 'Constitution diagrams' are used to predict ferrite levels from the composition by comparing the effects of austenite and ferrite stabilising elements. The Schaeffler and Delong diagrams are the original methods of predicting the phase balances in austenitic stainless steel welds. Nickel and chromium equivalents A 'nickel equivalent' is calculated for the austenite stabilising elements and a 'chromium equivalent' ferrite stabilising elements. These are used as the axes for the diagrams, which show the compositional equivalent areas where the phases austenite, ferrite, martensite (and mixtures of these) should be present. Although intended to show the phase balance of weld fillers, these diagrams can also be used to illustrate the phase balance of the 'parent' material. There are different diagrams for dif...