Dear sir,
Can anybody suggest GTAW consumables equivalent to AWS E10018-D2 and E 11018M?
Thanks and regards,
For Arc Welding Company,
Anil Verma
9999200148
Materials selection, welding, forming, Heat treatment, corrossion, NDT
Dear sir,
Can anybody suggest GTAW consumables equivalent to AWS E10018-D2 and E 11018M?
Thanks and regards,
For Arc Welding Company,
Anil Verma
9999200148