Hi,
I would like to know what weld size we should consider for Asymmetric fillet weld (a fillet weld where the legs are of unequal length). Please look at the attached file and let me know the weld size for ( 6 X 14 ) Fillet during welding at shop.
( 6 X 14 ) , is for example only , in reality it could be any uneven size like (... X ... ). Let me know if there is any standard procedure / thumb rule to consider the fillet weld size for this type of asymmetric callout.
Don't consider it may come as a welding process defect. It is from actual fabrication job and for illustrative purpose only.
Thanks in advance,
Joy
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Subscribe to:
Post Comments (Atom)
Re: [MW:35686] HDPE WPS
Refer ASME SEC IX There is separate chapter for Plastic welding . Based on that you have to prepare Sent from my iPhone On 21 Jun 2025, at...
-
Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? ...
-
Definition of buttering from ASME Section IX, QW/QB-492 Definitions: Buttering: the addition of material, by welding, on one or bot...
-
Section I. PRINT READING 3-1. GENERAL a. Drawings . Drawing or sketching is a universal language used to convey all necessary information to...