Thanks for your valuable inputs but EN 10204 is not saying about which tests to be witnessed. Are all tests to be witness, listed in product specification or only those which are given/confirm by customer..??
With Warm Regards,
Bhavesh Hansora
-----------------------------------
From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of dhilipkumar.m2010@gmail.com
Sent: Thursday, June 21, 2012 8:58 PM
To: materials-welding@googlegroups.com
Subject: Re: [MW:14639] 3.2 certification
Kindly refer the code EN 10204 for detail regarding 3.2 certification. Hope this will clarify your doubts.
Regards
M.Dhilip kumar
Sent from my HTC
----- Reply message -----
From: "MM" <rmuthusgs@gmail.com>
To: <materials-welding@googlegroups.com>
Subject: [MW:14623] 3.2 certification
Date: Thu, Jun 21, 2012 12:50 am
Dear Bhavesh Hansora
Has to witness what are all the tests given in that product specifications
Hope this will give a clear idea
Cheers
MM
From: materials-welding@googlegroups.com
[mailto:materials-welding@googlegroups.com] On Behalf Of Muthusrinivasan
Muthuselvam
Sent: Wednesday, June 20, 2012 9:02 AM
To: materials-welding@googlegroups.com
Subject: Re: [MW:14606] 3.2 certification
chemical & mechanical test as per relavant material specification.. In some
cases supplementary test called in technical delivery condition also has to
be witnessed by nominated third party inspector.
On Wed, Jun 20, 2012 at 9:52 AM, <Bhavesh.Hansora@dnv.com> wrote:
Dear One,
Can I know what is the requirement for 3.2 certification ??
Which are the tests to be witness by inspector ?
Bhavesh Hansora
-----------------------------------
****************************************************************************
********** The contents of this e-mail message and any attachments are
confidential and are intended solely for the addressee. If you have received
this transmission in error, please immediately notify the sender by return
e-mail and delete this message and its attachments. Any unauthorized use,
copying or dissemination of this transmission is prohibited. Neither the
confidentiality nor the integrity of this message can be vouched for
following transmission on the Internet.
****************************************************************************
**********
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to
materials-welding+unsubscribe@googlegroups.com
<mailto:materials-welding%2Bunsubscribe@googlegroups.com>
For more options, visit this group's bolg at
http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and
meant for educational purposes only, Users must take their own decisions
w.r.t. applicable code/standard/contract documents.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to
materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at
http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and
meant for educational purposes only, Users must take their own decisions
w.r.t. applicable code/standard/contract documents.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
************************************************************************************** The contents of this e-mail message and any attachments are confidential and are intended solely for the addressee. If you have received this transmission in error, please immediately notify the sender by return e-mail and delete this message and its attachments. Any unauthorized use, copying or dissemination of this transmission is prohibited. Neither the confidentiality nor the integrity of this message can be vouched for following transmission on the Internet. **************************************************************************************--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Comments