Dear Prakash,
 
Yes it is advisible to do cold forming on titanium.
Precauions:
 
1) Cut edges should be free from oxides/any other impurity.
2) While forming use SS liner in between the die & base metal.
3) Use more no of strokes while pressing because Ti has high spring back action.
4) If any crack occured, repair it by welding, no issue
 
Do not go for hot forming.

Regards,

Zakir Ali.


From: Prakash Hegde <pb.hegde@yahoo.com>
Sent: Thu, 21 Jun 2012 18:09:54
To: materials-welding@googlegroups.com
Subject: [MW:14614] Titanium Dished End Forming
Dear Friends
I have aquerry about Titanium Gr 2 material D/E of 10mm thk forming
i) What are the precautions to be taken during Forming of Titanium Dished End in cold to avoid crack
b) Is it advissible to form in cold?
ii) If it is to be formed in Hot condition what is a recomended temp and what should be treatment require to be given after forming i.e. renormalising  If so , is it required to foerm in Controlled atmosphere
 
Regards
 
Hegde P.B.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.


Follow Rediff Deal ho jaye! to get exciting offers in your city everyday.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...