Re: [MW:14649] 3.2 certification

 
Suppose Party A ( End User) gives Order of particular item (Example Pressure Vessel) to Party B (Turn Key Contractor)
 
Party B Gives Order to Party C (Sub Contractor, Mfg. of Pressure Vessel)
 
Party C gives order to Party D (Manufacturer of Fittings intended to be used in Pressure Vessel).
 
In this case can a party C inspection representative carry out required inspection at Party D ( Mfg.) and certify 3.2 certificate for a fittings?
 
Is it Posssible ?
 
 
Type 3.2 Inspection CertificateA document issued and validated by the manufacturer's independent and authorized inspection representative with an independent authorized representative of the purchaser and or third party inspector agency validation in accordance with the Specifications of the order.

On Wed, Jun 20, 2012 at 9:52 AM, <Bhavesh.Hansora@dnv.com> wrote:

Dear One,

 

Can I know what is the requirement for 3.2 certification ??

 

Which are the tests to be witness by inspector ?

 

 

Bhavesh Hansora

-----------------------------------

 


************************************************************************************** The contents of this e-mail message and any attachments are confidential and are intended solely for the addressee. If you have received this transmission in error, please immediately notify the sender by return e-mail and delete this message and its attachments. Any unauthorized use, copying or dissemination of this transmission is prohibited. Neither the confidentiality nor the integrity of this message can be vouched for following transmission on the Internet. **************************************************************************************

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...