Hi Friends,
I think ZT means, Z direction Through Thickness tested.
Please clarify again.
Cheers,
Saravanan,
Saravanan,
Korea
On Thu, Jun 28, 2012 at 5:57 PM, Kavin Murugam <kavin202082@yahoo.com> wrote:
Dear Venkat,Kindly refer SA20 ASME Sec II Part A.MT=Heat treatedLTV=CVN done.ZT= no ideaKavin Murugam0126159644From: "g.venkatesan06@gmail.com" <g.venkatesan06@gmail.com>
To: "materials-welding@googlegroups.com" <materials-welding@googlegroups.com>
Sent: Thursday, June 28, 2012 2:29 AM
Subject: [MW:14709] Explanation of MTLTV ZT-Reg
Dear sir.
I saw one carbon steel MTC SA 537 CL 1 MTLTV ZT.
What is the explanation of MTLTV ZT.
Which source or code gives that explanation.
Kindly guide me.
Regards
venkat
trichy
----------
Sent from my Nokia phone
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Comments