Re: [MW:14688] 3.2 certification


If Supplier is producing EN10204 3.1 certificate along with ISO 9001 then 3.2 certification is not required



From: Rana Vikas <vhrana@gmail.com>
Sent: Mon, 25 Jun 2012 14:16:05
To: materials-welding@googlegroups.com
Subject: Re: [MW:14670] 3.2 certification
Dear All,

3.2 Certificate include Physical & chemical testing result validated by independent third party nominated by purchaser.

Be Noted that 3.2 certificate with impact test is mandatory requirements for all CE /PED equipments. Its validated by NoBo ( Notified body).


Regards,
Vikas Rana

 

On Fri, Jun 22, 2012 at 8:27 PM, Vino Varghese <vinopvarghese@gmail.com> wrote:
Dear Bhavesh,
 
Can I understand the product for which you require a 3.2 Certification? The EN 10204 do not state the specific test requirement. I recommend to have a specific Inspection Test Plan which is agreed and accepted by Client to avoid any ambuigity at later stage. The supplementary requirements of any product standard(Eg: SA 106, witness of IGC test for SS material, witness of hardness etc, NDE requirements etc....)  could be a project specific requirement which might have to be included in the Quality Plan.
 
Hope the above give more light to the subject.
 
Regards
Vino-Doha  

On Fri, Jun 22, 2012 at 8:32 AM, <Bhavesh.Hansora@dnv.com> wrote:

Thanks for your valuable inputs but EN 10204 is not saying about which tests to be witnessed. Are all tests to be witness, listed in product specification or only those which are given/confirm by customer..??

 

With Warm Regards,

 

Bhavesh Hansora

-----------------------------------

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of dhilipkumar.m2010@gmail.com
Sent: Thursday, June 21, 2012 8:58 PM
To: materials-welding@googlegroups.com
Subject: Re: [MW:14639] 3.2 certification

 

Kindly refer the code EN 10204 for detail regarding 3.2 certification. Hope this will clarify your doubts.
Regards
M.Dhilip kumar

Sent from my HTC


----- Reply message -----
From: "MM" <rmuthusgs@gmail.com>
To: <materials-welding@googlegroups.com>
Subject: [MW:14623] 3.2 certification
Date: Thu, Jun 21, 2012 12:50 am


Dear Bhavesh Hansora

Has to witness what are all the tests given in that product specifications



Hope this will give a clear idea



Cheers

MM









From: materials-welding@googlegroups.com
[mailto:materials-welding@googlegroups.com] On Behalf Of Muthusrinivasan
Muthuselvam
Sent: Wednesday, June 20, 2012 9:02 AM
To: materials-welding@googlegroups.com
Subject: Re: [MW:14606] 3.2 certification



chemical & mechanical test as per relavant material specification.. In some
cases supplementary test called in technical delivery condition also has to
be witnessed by nominated third party inspector.







On Wed, Jun 20, 2012 at 9:52 AM, <Bhavesh.Hansora@dnv.com> wrote:

Dear One,



Can I know what is the requirement for 3.2 certification ??



Which are the tests to be witness by inspector ?





Bhavesh Hansora

-----------------------------------




****************************************************************************
********** The contents of this e-mail message and any attachments are
confidential and are intended solely for the addressee. If you have received
this transmission in error, please immediately notify the sender by return
e-mail and delete this message and its attachments. Any unauthorized use,
copying or dissemination of this transmission is prohibited. Neither the
confidentiality nor the integrity of this message can be vouched for
following transmission on the Internet.
****************************************************************************
**********

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to
materials-welding+unsubscribe@googlegroups.com
<mailto:materials-welding%2Bunsubscribe@googlegroups.com>
For more options, visit this group's bolg at
http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and
meant for educational purposes only, Users must take their own decisions
w.r.t. applicable code/standard/contract documents.



--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to
materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at
http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and
meant for educational purposes only, Users must take their own decisions
w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.


************************************************************************************** The contents of this e-mail message and any attachments are confidential and are intended solely for the addressee. If you have received this transmission in error, please immediately notify the sender by return e-mail and delete this message and its attachments. Any unauthorized use, copying or dissemination of this transmission is prohibited. Neither the confidentiality nor the integrity of this message can be vouched for following transmission on the Internet. **************************************************************************************

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.


Follow Rediff Deal ho jaye! to get exciting offers in your city everyday.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...