Dear All ,

Is there any minimum thickness limit specified in any code for the
tubesheet plate UT check to be carried out.
Normally, almost code did not mention about min thickness limit.
But so far, you can refer AWS D 1.1, 6-Part F: "For thicknesses less than
5/16 in. [8 mm] or greater than 8 in. [200 mm], testing
shall be performed in conformance with Annex S", you can refer Annex S in special case. So, in normal case, min thickness is 8mm.
Or other code you can refer: EN1712 (EN 11666) limits the checks welds to 8mm; EN 10160 limits to 6 mm the plates control; ISO 12094 go down to 4 mm
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...