Dear Pradip Sir,

Thank you very much for your valuable information. Still some doubts
are there as given below.

As per AWS D10.10( Clause2.3.1)temperature variation up to 83deg is
acceptable and AWS D10.10 itself says that there is no way to
eliminate temperature variation though out the wall thickness(Clause
2.3).

Actually in our site we have materials with various thicknesses and
some up to 139mm and now question is.. what will be the temperature
variation for 139mm thickness(On jobs its not possible to measure
inside temperature).

Have any equation or formula to find out the temperature variation
throughout the thickness?

Have any role of Thermal conductivity of P91 in this case?

Is it possible a uniform temperature at OD and ID regardless of
thickness?

Awaits for your reply

Thanks and regards

Sandeep
QC Engineer

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...