Thursday, March 22, 2012

Re: [MW:13971] Filler for Monel to carbon steel

Dear

ErNiCu1 or ERNiCu7 both are compitible. Preheat CS to atleast 75 deg c to avoid any cracking.


VJ

On Thu, Mar 22, 2012 at 10:57 PM, Dsunil <dsunil@gicongoa.com> wrote:

Dear Experts,

 

Can  you recommend thet filler in ER series  for welding  Monel 400  to  Carbon Steel (A105)  material.

 

Thanks and regards

S G Dixit

Sr. Manager- Materials

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...