Wednesday, March 21, 2012

Re: [MW:13965] TENSILE TEST REQUIRMENT FOR PLATES AFTER SIMULATION HEAT TREATMENT

If heat No.is same do test on 1 plate.
 
Thanks & Regards,

(Karthik)

Karthikeyan.S
QA/QC Manager
German-Thai Boiler Engineering Cooperation Limited.
Rayong Factory ;
379 Moo.6 Soi 8, Tambol Pananikom,
Nikompattana, Rayong 21180 THAILAND
Tel : +66 38 897 035-9 Ext. 137
Fax : +66 38 897 034
Hand Phone: 0066 892512282

From: asad azmi <azmiasadayub@gmail.com>
To: materials-welding@googlegroups.com
Sent: Wednesday, March 21, 2012 6:26 PM
Subject: [MW:13963] TENSILE TEST REQUIRMENT FOR PLATES AFTER SIMULATION HEAT TREATMENT

Dear All,
 
A vessel is being fabricated as per ASME SEC VIII DIV 1.
 
 
Contarctor has received 3 plates ( SA 516 GR 70 N - 30 mm Thk) which are having one heat number and 3 different Plate No. Plate condition - Plate Hot Rolled. plate manufacturer has not done Simulation heat treatment of test coupon.
 
as per Client  Simulation  heat treatment ( 3 pwht cycle) is reuired. 
 
As per SA 20 PARA 11.1.1 One tension test is required for each plate as rolled. as per client requirment any mechanical testing shall be done after all heat treatment.
 
 
Please advice whether one sample from each plate has to undergo simulation heat treatment cycle & Tension test OR one sample out of any 3 plates shall undego simulation heat treatment & Tension Test.( as heat number is same for each 3 plates)
 
Please give code reference.
 
Thanks & Regards
 
Asad Azmi
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.


No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...