[MW:13993] RE: 13973] If a welder is qualified in CS - GTAW process, Is the same welder can weld SS - GTAW process with purging ?

Yes

 

See QW-356 and QW-404.15 for filler metal  (Same F-number, F6)

And

See QW-356 and QW-408.8 for backing gas.  (Qualification w/ backing gas qualifies only with backing gas, qualifying w/o backing gas qualifies both w/ and w/o)

 

John A. Henning

Welding & Materials

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of mpk mpk
Sent: Thursday, March 22, 2012 11:08 AM
To: materials-welding
Subject: [MW:13973] If a welder is qualified in CS - GTAW process, Is the same welder can weld SS - GTAW process with purging ?

 

Dear Experts,

 

If a welder is qualified in CS - GTAW process, Is the same welder can weld SS - GTAW process with purging ?

 

Thank you,

MPK

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.


______________________________________________________________________
The information in this email is confidential, and is intended solely for the addressee(s). If you are not the intended recipient of this email please let us know by reply and then delete it from your system; you should not copy this message or disclose its contents to anyone. The internet can not guarantee the integrity of this message. HAMON (and its subsidiaries) shall (will) not therefore be liable for the message if modified.
______________________________________________________________________

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...