Friday, March 30, 2012

[MW:14026] Re: PWHT OF P91 BY INDUCTION HEATING

Dear Pradip Sir,

Thank you very much for valueble informations. We are going to conduct
another PWHT mock test,considering all these facts and skilled
technicians have been called for the same.

Regards,


Sandeep