Use ERNiCu-7 ….. It can also be used for joining these alloys to steel. usually welded with pure Ar as the shielding gas.
Eng. Ahmed Osman
Senior QA/QC Eng.
Orascom Construction Egypt
+20 122 5880434
ahmed.mahmoudmohamed@orascomci.com
a.osman81@yahoo.ca
From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Dsunil
Sent: Thursday, March 22, 2012 7:28 PM
To: materials-welding@googlegroups.com
Subject: [MW:13970] Filler for Monel to carbon steel
Dear Experts,
Can you recommend the filler in ER series for welding Monel 400 to Carbon Steel (A105) material.
Thanks and regards
S G Dixit
Sr. Manager- Materials
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Comments