Hi,
The profile comparator is the normal practice done in painting inspection.If you want to buy Surface roughness measuring instruments,there are lot of manufacturers available in the market like Mitutoyo,kosako etc.,
 
Thanks & Regards,

(Karthik)

Karthikeyan.S
QA/QC Manager
Getabec Energy Co.,Ltd.
379,Moo6,Soi8,Nikhomphatana,
Rayong-21180,
Thailand.
Phone: 0066 38 897035-8 (Off)
Fax: 0066 38 897034
Hand Phone: 0066 892512282


From: Vasantharao <vasantharao@yahoo.in>
To: "materials-welding@googlegroups.com" <materials-welding@googlegroups.com>
Sent: Thursday, December 22, 2011 5:08 PM
Subject: [MW:13256] Surface roughness measurement instruments.

Dear Experts,

I work as inspection Engineer. When i go for Blasting inspection, contractor provided  me profile comparator for surface roughness measurement.

Contractor do  Grit blasting in the shop.

I need to measure surface roughness  -  75-100 microns      Painting system No#1
                                                            50-75 microns        Painting system No#2

Queries


Q 1: Comparator is enough for surface roughness measurements.

Q2: Is any other tools available for roughness measurement?.

Q3:  What is the normal industry practice.


Pl. provide your valuable suggestions as i'm new for painting activities.

Rao.


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.


No comments:

[MW:35738] ASME IX WPS Qualification Query: GTAW + FCAW with Multiple PQRs

Dear Welding Experts, I'm currently preparing a Welding Procedure Specification (WPS) and have encountered a request to qualify a GTAW +...