Re: [MW:13279] Identification of thickness on Radiography films.

Dear Sir
Construction code is ASME B31.3(Power Cycle Piping)
But as per my vendor, the selection of penetrometer is the total thickness including reinformcements of the welds.So, based on the thickness the weld reinforcment varies, so vendor argues that it can create confusion(only in border cases) if wall thickness is mentioned in the film.
Generally, the film identification shall be placed on the film to make a corelation with the report & to fullfill the mandatory requirements as laid down by the code.
Kindly advise.
----- Original Message -----
From: george dilintas <george.dilintas@gr.bureauveritas.com>
To: materials-welding <materials-welding@googlegroups.com>
Sent: Thu, 22 Dec 2011 23:42:07 +0530 (IST)
Subject: Re: [MW:13269] Identification of thickness on Radiography films.

Which is your construction code?
Best regards
Dr Georgios Dilintas
Authorized Nuclear Inspector
Authorized Inspector Supervisor
HBS Regional Technical Manager


----- Original Message -----
From: Ramchandra vichare [vicharerke@indiatimes.com]
Sent: 22/12/2011 16:29 ZE5B
To: materials-welding@googlegroups.com
Subject: [MW:13257] Identification of thickness on Radiography films.

Dear Experts,

During Interpreting Radiography films at one of my vendor's works, I observed that, there is no identification /indicate thickness of job on film so I rejected the film. As far as generally everyone related field experience persons are know unless identification of thickness on film it is very difficult to know which penetrameter to be used but my vendor is arguing for the same. According to him one of "Level III" person insisit them there is no need to mentioned thickness in Radiography films and it sufficient if it indicate in Radiography interpretion report.
Suppose in piping number of joints/piping spools are comming with verious thickness in same report in such case it is possible to identify required penetrameter ? My anser is no, each Radiography films must be indicat thickness of joint/job. Requested to suggest/advise.

Sincerely yours,
RK Vichare

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...