Re: [MW:13368] Re-expansion of tubes for Air Fin Cooler.........

Yes ..I agreed with Mr. Izad  ....

Suresh


On Thu, Dec 29, 2011 at 1:57 PM, hizad idris <hizad.idris@gmail.com> wrote:
Dear Vinod,
 
If still leaking after re-expand, my suggestion to plug off the tube, if the performance still within the required coolers performance. Normally , cooler have over design up to 20%. Need to calculate the cooler performance with the remaining tube, after plug off.

-izad-
 
On Wed, Dec 28, 2011 at 9:40 AM, Vinod Jotwani <poojvin@yahoo.com> wrote:
Dear Experts,
 
We have one of our fin fan cooler leaking from tube to tubesheet joint. The tube material is Duplex stainless steel.
 
We would like to carry out re-expansion of the tubes, your advise is needed for %age expansion allowed when these tubes are to be re-expanded. The tubes are in operation since last one year in Sour Water Recovery Unit ( H2S service).
 
Also if some body can share their experience in case of leakage even after re-expansion how to repair the tube to tube-sheet joint. For information the header is welded constuction.( Ref attached file )
 
 
Thanking you,
 
Vinod
 
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
Thanks  & Best Regards,

Suresh

Mobile No: 91-92 92 905 905

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...