[MW:13361] RE: 13356] welding P355NL2

Dear Sir,

 

P355NL2 is low carbon steel for pressure vessels at low temperature applications, material delivered according to EN 10028-3 (Flat products made of steels for pressure purposes - Part 3:

Weldable fine grain steels, normalized). As the title of the material specification already mentions it has good welding properties like all low carbon steels because of low carbon content (<0,18%).

All welding processes are possible, you only have to take care about layer thickness and heat input during welding in case you need high impact values at low temperature. We normally weld this material with a standard SG3 type solid welding wire (GTAW / GMAW / SAW).

 

Met vriendelijke groeten / Best Regards

 

Herman Pieper

 

Pieper Quality Support & Inspection

Phone: +31 (0)521 380083

Fax:     +31 (0)84 7539225

Cell:     +31 (0)6 51691215

www.pieper-qsi.nl

 

Van: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] Namens Himan Nikdin
Verzonden: woensdag 28 december 2011 18:08
Aan: materials-welding@googlegroups.com
Onderwerp: [MW:13356] welding P355NL2

 

Dear Experts

 

would you please share some information about welding P355NL2?

 

Regards

Himan Nikdin

--
To post to this group, send email to
materials-welding@googlegroups.com
To unsubscribe from this group, send email to
materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at
http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...