yes it is required, you can use Argon gas.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
On Sat, Dec 24, 2011 at 11:39 PM, prem nautiyal <prem_nautiyal26@yahoo.com> wrote:
Hi friendsI am establishing a welding procedure for welding of 90-10 Cu-Ni 6mm thick tubes, UNS C70600 as per ASME SecIX.All joints are single sided joints and i will be welding them with TIG: ER CuNi filler wire.My only query was that do i need to back purge the weld joints ?RegardsPrem S Nautiyal
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.