Dear Rao,

My suggestion follows:-

(1) Surface comparator is sufficient as in your spec must have mentioned about roughness grade Sa 1, Sa2, Sa2.5 or Sa3 which is equivalent to 75-100 micron or what so ever accordingly you can compare. 

(2)Dial depth gauge and Testex Replica film for permanent record are available.

(3)In your case Testex Replica film is the normal industrial practice. 

Thanks from
Saravanan Mohan


On Fri, Dec 23, 2011 at 1:59 AM, yogeshkumar Kumbhar <kumbharyogeshv@gmail.com> wrote:
Dear Member,

Please find attached file profile depth micrometer for measuring microns.






On Thu, Dec 22, 2011 at 3:38 PM, Vasantharao <vasantharao@yahoo.in> wrote:
Dear Experts,

I work as inspection Engineer. When i go for Blasting inspection, contractor provided  me profile comparator for surface roughness measurement.

Contractor do  Grit blasting in the shop.

I need to measure surface roughness  -  75-100 microns      Painting system No#1
                                                            50-75 microns        Painting system No#2

Queries


Q 1: Comparator is enough for surface roughness measurements.

Q2: Is any other tools available for roughness measurement?.

Q3:  What is the normal industry practice.


Pl. provide your valuable suggestions as i'm new for painting activities.

Rao.


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
With Best Regard's


Yogesh V Kumbhar

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...