Dear sir,
Please Find the Below Answer In Green.
On Thu, Dec 22, 2011 at 2:08 PM, Vasantharao <vasantharao@yahoo.in> wrote:
--Dear Experts,I work as inspection Engineer. When i go for Blasting inspection, contractor provided me profile comparator for surface roughness measurement.Contractor do Grit blasting in the shop.I need to measure surface roughness - 75-100 microns Painting system No#150-75 microns Painting system No#2
QueriesQ 1: Comparator is enough for surface roughness measurements.Q2: Is any other tools available for roughness measurement?. For measuring the roughness as per SA 2 1/2, we can measure with help of Press " O " Films, With help of Dail Gauge we can Measuring the microns in a Press "O" Flim. Minus -50 microns from absorved to get actual valve. After blasting with in 3hrs primer to be painted.Q3: What is the normal industry practice.
Pl. provide your valuable suggestions as i'm new for painting activities.
Rao.
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Comments