Dear Mr Martin,

As we done here SDSS fabrication we are
following client Spec, Only up to completion of root pass, Oxygen
level shall be below -100 ML/Ml3, During welding if exceed 500 Ml/Ml3
then welding has to stop,this process follow up to three layer.

Depending upon you thickness of deposit. After three layer heat input
cannot oxidize the root, It optional u can maintain up to 10 mm thick
welding ,if pipe thickness is more than 10mm u can stop backing gas .


Regards

Madhu


On 12/28/11, Martin Prad <martin_prad@hotmail.com> wrote:
>
> Hi friends,
>
> I have 2 different specification which the requirements are different for
> the oxygen level in purging gas during the welding of super duplex pipe.
>
> One of them calls for 25 ppm (0.0025%) another one calls for 5000 ppm
> (0.5%). Could you please shed some light on this as which one is up to the
> standard with references?
>
> Thanks,
> Martin.
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to
> materials-welding+unsubscribe@googlegroups.com
> For more options, visit this group's bolg at
> http://materials-welding.blogspot.com/
> The views expressed/exchnaged in this group are members personel views and
> meant for educational purposes only, Users must take their own decisions
> w.r.t. applicable code/standard/contract documents.
>

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...