Re: [MW:13280] Surface roughness measurement instruments.

Dear Mr.Jagath,

Thank you for providing valuable info.

I do inspection of Off-shore platforms.

At present Blasting & painting of Jacket legs are in progress and Copper slag is the abrasives used for blasting.

Contractor use "G" type comparator  & its roughness values are attached for info.

I have still ambiguity regarding  tools to be used for roughness value.

my main question is what is the industry practice & is it comparator more than enough for surface roughness measurement?

best regards

Rao


From: jagath kavali <jagath.kavali@gmail.com>
To: materials-welding@googlegroups.com
Sent: Thursday, 22 December 2011 7:30 PM
Subject: Re: [MW:13264] Surface roughness measurement instruments.

Dear vasantha rao,

    For surface roughness measurement comparator is sufficient, You are not specified the type of equipment & application of the equipment.

For surface roughness measurement Digital and dial gauges available in the market we are using the same.

By using the comparator you could not get the exact  value of the roughness , Comparator is not sufficient for all kind of jobs.


Best regards

Jagath

On Thu, Dec 22, 2011 at 3:38 PM, Vasantharao <vasantharao@yahoo.in> wrote:
Dear Experts,

I work as inspection Engineer. When i go for Blasting inspection, contractor provided  me profile comparator for surface roughness measurement.

Contractor do  Grit blasting in the shop.

I need to measure surface roughness  -  75-100 microns      Painting system No#1
                                                            50-75 microns        Painting system No#2

Queries


Q 1: Comparator is enough for surface roughness measurements.

Q2: Is any other tools available for roughness measurement?.

Q3:  What is the normal industry practice.


Pl. provide your valuable suggestions as i'm new for painting activities.

Rao.


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.


No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...