Thick carpet material can be pasted on the CS Roller for SS Plate rolling to avoid direct contact of CS. Periodic inspection is required to ensure no damage of carpet during rolling. The same time CS plate cannot be rolled with same carpet for other job which may contaminate with carbon steel.

 

M.M

  


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Ariel
Sent: Wednesday, December 28, 2011 11:10 AM
To: materials-welding@googlegroups.com
Subject: RE: [MW:13346] Stainless steel plate rolling

 

I would not  be gluing anything to the roller. That would open the door for  possible worse problems such as out of shape rolling. 

 

I would maintain the integrity of the roller and would passivate S/S upon completion of vessel, to ensure that the environment ( C/S workshop fabrication) it has been worked on did not affect/contaminate the material’s anti-corrosive properties .

 

Ariel

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Lassaad Mokrani
Sent: Wednesday, 28 December 2011 3:04 AM
To: materials-welding@googlegroups.com
Subject: Re: [MW:13338] Stainless steel plate rolling

 

Yes this is the only one precaution to take.

It could be even a kind of a temporary glued thin matela

2011/12/27 rinshu <rinshad043@gmail.com>

Dear all,


Can anybody help me on the rolling of austenitic stainless steel plate
for the pressure vessel,we are having facilities for the rolling of
carbon steel plate. Can we use the same rolling machine? Need to have
any precaution before rolling in the same machine ?


Regards

Rinshad

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.




--
Meilleures salutations

Mokrani Lassaad
00216 20 649 755
http://www.linkedin.com/pub/lassaad-mokrani/16/364/907


















P     Pensez environnement! N'imprimez ce mail que si c'est vraiment nécessaire
Please consider your environmental responsibility before printing this e-mail


This e-mail is confidential and it is intended only for the addressees. Any
review, dissemination, distribution, or copying of this message by persons
or entities other than the intended recipient is prohibited. If you have
received this e-mail in error, kindly notify us immediately by telephone or
e-mail and delete the message from your system. The sender does not accept
liability for any errors or omissions in the contents of this message which
may arise as a result of the e-mail transmission

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...