After welding, less than 1.5 mm gap is the cause to reject the weld after
RT?
If yes, in accordance which criteria?

Thanks...

Nebi ÖZHAN

e-mail:nozhan@cimtas.com.tr
--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

1 comment:

Anonymous said...

The gap needs to be 1.5mm before welding. The gap is there to prevent stress on the weld or parent material from expansion from heat.

If it is rejectable, i haven't seen the code yet that says so. Although it may be a customer requirement that there is some gap after welding to ensure that undue stress did not happen