We want to weld a 24'' SS PIPE A358 GR 321, 6.53 mm THK, to a Fitting / Pipe with same size and specification but with a Thickness of 9.53mm and 12.70 mm.

Can we do the welding of these items? What is the accepted tolerance as per ASME B31.3? Where can I find these details in ASME B313.3?