[MW:834] Re: Friction Stir Welding

If you want to know more about it, go to http://www.msm.cam.ac.uk/phase-trans/2003/FSW/aaa.html .
 
Regards,
Owen Jenkins.
----- Original Message -----
Sent: Sunday, June 08, 2008 4:24 AM
Subject: [MW:833] Re: Re; STI welding

Friction-stir welding (FSW) is a solid-state joining process (meaning the metal is not melted during the process) and is used for applications where the original metal characteristics must remain unchanged as far as possible. This process is primarily used on aluminum, and most often on large pieces which cannot be easily heat treated post weld to recover temper characteristics. It was invented and experimentally proven by Wayne Thomas and a team of his colleagues at The Welding Institute UK in December 1991. TWI holds a number of patents on the process, the first being the most descriptive.

Fly Yalung <fly_ma_alkawari@yahoo.com> wrote:
Does any one knows about STI WELDING info.


--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...