Re: [MW:35902] Request for Consumable Estimation Sheet for GTAW/SMAW Pipeline Welds


Parameter,Value
Joint Type,V_GROOVE
Material,CARBON_STEEL
Process,GMAW
Thickness (mm),10
Included Angle (deg),60
Root Gap (mm),2
Root Face (mm),1
Weld Length (m),1
Efficiency,0.92
Reinforcement (mm),2
---,---
Results,
Cross Section Area (mm2),79.16
Volume (cm3/m),79.16
Total Volume (cm3),79.16
Weight (kg/m),0.62
Total Deposit Weight (kg),0.62
Total Filler Required (kg),0.68
Dear  MD MASUD RANA
Please check it

With Regards,
M.Magesh kumar

On Wed, 19 Nov 2025 at 16:26, Masud Hamza <masudhamza14@gmail.com> wrote:

Hello everyone, I hope you are all doing well.

I am seeking technical assistance in developing a welding consumable estimation format for pipeline fabrication.
For reference, consider the following joint configuration:

  • Pipe Size: 16-inch

  • Wall Thickness: 12.7 mm (XS)

  • Welding Process: GTAW (root & hot pass) followed by SMAW (fill & cap)

I would appreciate a standardized consumable-calculation template—preferably in Excel or PDF—to accurately determine filler metal requirements, deposition rates, joint volume, and allowable tolerances for this type of weld.

Thank you in advance for your support and technical guidance.


Best Regards
MD MASUD RANA
QA-QC Inspector(Welding & Piping)
Mechanical Engineer.
Pipeliners Limited.
Bibiyana Optimization Project (Turbo Expander)
Contact NO: 01738-862988

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAN5jLqKkgmzagA_RDervEtaK_OCHw5LqfcpC7OdX5HGtDWuTfw%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CALABf26oNBJ8sxOhNEV8%3DMs-FVwGjpxFaR8pjMdRO25eO82SmA%40mail.gmail.com.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...