Skip to main content

Re: [MW:35874] Re: PWHT REQUITEMENT AS PER ASME Section VIII Div.1 UCS-56

UW-40.6 given how determined PWHT think. Base on that 50mm need to consider for PWHT.




From: materials-welding@googlegroups.com <materials-welding@googlegroups.com> on behalf of Mohmmed Dudhiyawala <mdudhiya007@gmail.com>
Sent: Monday, October 27, 2025 7:39:27 am
To: Materials & Welding <materials-welding@googlegroups.com>
Subject: Re: [MW:35872] Re: PWHT REQUITEMENT AS PER ASME Section VIII Div.1 UCS-56

Dear Bilal,
Refer to Sec VIII Div. 1, UW-40 (f)5f, the governing thickness for PWHT calculation for Non pressure # Pressure Part is the thickness of the weld at the point of attachment. Request calculate Soaking time as per the same.
From attached image, it is appearing as a Groove weld across the thickness. 

Regards,
Mohammed 

On Thursday, October 23, 2025 at 9:49:19 PM UTC+5:30 Prem Nautiyal wrote:
Please proceed with PWHT considering 50mm butt weld size thickness of Trunion ..

Regards

Prem Nautiyal 
Mumbai, India 

On Thu, 23 Oct 2025 at 21:05, Bala Murugan <balamur...@gmail.com> wrote:
Dear Bilal,
No, you cannot simply ignore the 50 mm trunnion when deciding PWHT. ASME VIII-1 (UCS-56 and related notes/interpretations) makes the pressure-retaining part control the PWHT temperature, but the thickness at the weld/attachment and the weld volume (soak band) are explicitly used to determine heating rate and holding/soaking time. In practice you must check UCS-56 and the ASME interpretations and use the greater thickness condition required by the Code rules for the weld/joint when sizing soak time (and ensure the soak band contains the weld and HAZ)  

Thanks,
Balamurugan

On Thu, Oct 23, 2025 at 8:38 PM Mohd Siraj <mohd...@gmail.com> wrote:
by sketch, its joint between 22mm and 50mm ?

so consider thickness 22mm butt weld and beyond above is fillet joint.

On Thursday, October 23, 2025 at 4:57:31 AM UTC+3 Ch Bilal jovinda wrote:
Dear Team,

  I want to confirm about the PWHT requirement in carbon steel pressure vessel as per ASME section Viii Div.1 UCS-56. Soaking time has been calculated as per vessel wall thickness 29mm but trunion wall thickness is 50mm welded with shell. Can this 50mm thikness be exluded from PWHT soaking time requirement. 
1.Is there any interpretation to confirm that PWHT parameters shall be calculated as per shell wall thickness only not for attachment welded with pressure parts?
2. Below para is applicable for PWHT requirement.




Best regards,
M Bilal

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/ed05ee2b-bc27-4391-82eb-32886ca2700en%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/cbbe8721-6b06-4945-bf72-8ac0699c9deen%40googlegroups.com.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...